Available for analysis of low-molecular-weight compounds
Compared to Inertsil ODS-2, pores are narrower, surface area is larger and carbon load is less. Theoretical plate number for low-molecular-weight compounds is high. Small molecules are retained on Inertsil ODS-80A longer than on Inertsil ODS-2.
Particle Size |
Particle Shape |
Surface Area |
Pore Size |
Pore Volume |
Bonded Group |
End-Capping |
Carbon Load |
pH Range |
5 µm |
Spherical |
450m2/g |
80Å |
0.80mL/g |
Octadecyl group |
Yes |
17.5% |
2 - 7.5 |